Governing thickness is as per B31.1 & 31.3 is Nominal material thickness??

On Sat, 4 Jan 2020 9:50 pm Tajuddin Mohammed, <tajuddinjntu@gmail.com> wrote:
Yes we need to do the  PWHT of these type of joints as it is directly welded to the pipe

Mohammed Tajuddin

On Sat, 4 Jan 2020, 6:07 pm Chiranjeevi A, <chiranjeevipuvvula@gmail.com> wrote:
Dear Raghuram Bathula,

   The main run pipe 20" is having thickness of 31.mm and being subjected to PWHT.
A dummy leg (12") is welded to the main pipe as dummy leg. pls confirm that, do we require PWHT at this joints as highlighted in below snap


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0zOsMaca5bYCPWfVvRa1kRdBWqgcGKGMNEXf_k_dMXzMg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACZrEUbwy%2BdLw1gP70k18Ox6iPs%3DngfQmjzpqYG9xiWw44kXCA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOCE4j5Tb80xvgijR5mXNnOHUsMuS_jdLXhT8fTOMxMOA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...