Wednesday, January 15, 2020

[MW:30384] WPS

dear Guy's,

GM

The WPS which is qualified with P1 Gr.2 with Clad Alloy 825 will qualify to weld P1 Gr.2 with Clad Alloy 625 to equivalent or same material…? required separate qualification for P1 Gr.2 with Clad Alloy 625 ?.


thanks in advance for your's prompt reply.


Babu 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9a533821-faa6-473e-be7f-15a39c2ffcc6%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...