Tuesday, December 24, 2019

Re: [MW:30319] PSV set pressure during hydrotest of piping

Dear Manoj,

Please check through API RP 520 and you should find the set pressure requirement for PRVs. Typically it is set based on the MAWP or  design pressure. However you also need to consider the static head between the protected equipment and the relied valve while deriving the set pressure.

Hope this helps.


Thanks and Regards
Vino



On Tue, Dec 24, 2019, 08:23 Manoj John <manojacgnr@gmail.com> wrote:
Dear Experts,

As per B31.3 what is the PSV set pressure during hydrotest.
Please give expert opinion as there is no clause found in B31.3 for hydrotest PSV set pressure, PSV set pressure for pneumatic only prescribed.

Thanks in advance,
Manoj

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACgUO5nJ9-S1uDxZVTxg%2BYRcsUy8F64M-QRiugW%2BKbmYx6s8Lw%40mail.gmail.co

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM7oz7DLt%2Bn_Rq50i7a7iLO7S2M%3D1V9N_128874eoR4%3DdzB8RQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...