Monday, December 23, 2019

Re: [MW:30310] Filler material Selection

Pl refer B31.1 , chapter V, 128 and give your opinion , when joining Austenitic material with other like C's, weldmetal structure should have Austenitic structure. Thanks

On Mon, 23 Dec 2019 4:35 pm 'anand gupta' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear 
If base metal is SA 106 GR B then why u r going for SS316L. 

Simple go for  ER70S2/E7018

REGARDS 
A P GUPTA 
BARODA 
THYSSENKRUPP 


On Mon, 23 Dec 2019 at 10:55, Navanith
Dear Experts,

Require guidance on filler material selection as per ASME BPVC.
For example:I received this query from a client
Base metal is ASTM A106 Gr.B and they want to weld using E316L electrodes.
Is it possible to use E316L electrodes to weld directly?

Regards,
Navanith

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/37bac14e-c9a8-4d35-af83-c5e116da3bc8%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1521750501.2203327.1577082216551%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNbKUU4BrPT4ndLc3mbP1saha9dJ2zCZC3%2Bj%2Bw8fFYb6w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...