[MW:30295] Re: Minor Cracks in SAW Welds Cap

Hello Gowtham Rajendran

You should try to preheat metal to min 75C deg. Because you're parameter very high and metal have to stress during welding and after welding it cooling.
Second question: could you show How are located welding seams on  construction.





2019 m. gruodis 17 d., antradienis 07:58:10 UTC+2, Gowtham Rajendran rašė:
Dear All,

In the cap pass of the SAW Welding, we have observed some minor cracks while performing MPI as you can find in the attached pics.

With pipes welded with the same parameters and almost the same condition, we are finding this kind of defect in some pipes, if anyone has come across such kind of defects, kindly share your experience and possible root cause.

Thanks in advance for your valuable inputs.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8a3fcdd-73d2-40d3-aa3b-4c81f0f8303e%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...