Dear experts,
For after weld cleaning of SS weld joints my client insisted to do buffing on all the joints.
1. Is it a good suggestion?
2. Is there any technical argument so that we can avoid it?
3. Will buffing remove the passive layer and promote corrosion?
4. I got a comment that Buffing is a pickling activity and it should follow the preparation of not better not to go for buffing.
Presently we are cleaning the joints with SS wire brush after welding.
We don't have pickling and application in the scope of work and no need to for the same.
Thanks in advance.
Regards,
Hareesh K V
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4f2d4a76-e9b3-4ab5-ae3a-27f98eab44d7%40googlegroups.com.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment