Tuesday, November 5, 2019

Re: [MW:30205] EPDM RUBBER SHEET VS BUTYL RUBBER SHEET

It's highly depends on the place of uses

On Mon, Nov 4, 2019, 16:44 Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear Experts,

  For cold insulation we have contraction joints where we use butyl rubber sheet used as external bellow. But cost effective we are using EPDM rubber sheet which is from same family and can be folded same as butyl rubber. 

Can we use EPDM, experts share you opinions

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0ysfi6TR3DVmpNoQMS%2BtO9E9uUAuvFV08v9_mhw0x8VWg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UOV-9rpBwCo_%2Bg4tvKgdcogaaCSzehUF1JFnFfotG84Wg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...