Re: [MW:30135] Distance between two weld joint

Dear Shiva

Please see your project specification ....Distance between weld join will varies as per Client standards... 

In general ..3 times of WT should be required ...

On Fri, Oct 4, 2019 at 4:19 PM siva Guru <dhanaguru2010@gmail.com> wrote:
Dear All
Can you advice, 
two weld  joint how much Min distance between weldjoints.
Please clarify, if possible please provide code reference.

Best regards

Guru

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEDN%2BXFp1f7duhV4NFBmu_87QNzsuA877q4wDUTDuEOPTOM7eQ%40mail.gmail.com.


--
Thanks  & Best Regards,

Suresh Paidi


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA%3D1_-xKu7x6yV9zVTcMj1PX6Q32wLM%3DeyJGbYm8EzmjFK0EkQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...