Re: [MW:30033] Welder qualification

If welder do welding on less than minimum 73 mm OD of pipe He able to qualify on minimum  1" pipe 25 mm OD pipe. Below 1" welder will have to do test on whatever doa required.


Kind Regards,
Mohit Aggarwal



On Sat, Aug 31, 2019, 00:23 Raghul <raghul351991@gmail.com> wrote:
Welder made two coupon
1. Coupon with 6 mm thickness on the 1/2" pipe made by gtaw process
2.coupon with 15 mm thickness on 2-7/8" pipe made by gtaw+smaw process.

Is the welder qualify to weld on 1/2" pipe with gtaw+smaw process for qualified thickness?

Please explain

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4a02db6d-d531-4b87-a6be-76c6bfa924e1%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPN6tS9jqR03_jQxEqVkZS0yCvnKCtaYyqYkG-vT1dRpXQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...