Gents,

I simulation heat treatment required for material sample if the equipment not required impact test as per UCS-85 of ASME SEC VIII?




Thanks & RegardsMuhammed Ibrahim PK


On Wed, 18 Sep 2019 at 15:50, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:
Gents, 

Is simulation heat treatment required for material as per latest ASME sec viii?.

Reg, 
Ibrahim





Virus-free. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmOXL5hNUSoRJ9ick19L0g%3D9m_%3D7TkH8cFxqh2x%3D%2BtXsOA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...