Monday, August 5, 2019

Re: [MW:29924] How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.

Dear,

One coupon is enough, as the length required  for radiography is 150mm,

Regards, 
Anthony 

On Mon, 5 Aug 2019, 17:40 'Raja kumarasamy' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear sirs,

How many coupons needed for welders qualifications of welder from 2'' (OD:60.33 mm) SCH : 5.18 mm ) GTAW according to ASME SEC.IX.




Regards 

 

Raja kumarasamy
Welding & Piping inspector
ADNOC Waste Heat Recovery Project
Ruwais, Abudhabi
UAE  Mobile:  +971-565495293
INDIA  Mobile:  +91-9487403889


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1308484406.1069275.1565010887764%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOi%3DZp9NERmJXn%2B1_n36%3DBuB8Wt%2B3BMyxEso9z_Ea3v2rY6ijA%40mail.gmail.com.

No comments: