Thursday, July 18, 2019

Re: [MW:29860] Asme Section IX Thickness range qualification

Thanks for the feedback

Yes, snap is ready WPS, follows attached.

But according to QW-451 because the coupon thickness is 25.4mm, the qualified range would be 5 to 2T, regardless of having deposited only 8mm with the GTAW process?

Thanks.

Isac

Em quarta-feira, 17 de julho de 2019 04:37:57 UTC-3, Muneeb escreveu:
Yes you can, 

Your 25.4 mm with gtaw and smaw can write 2t ranges from your PQR for what has been deposited individually.

you are going to write a WPS or below snap is ready WPS?

Check impact / PWHT requirements for what you qualified and what recommended in production joint.

Thanks.
Mohamed Muneeb Mahaboob.
 
Date: 2019-07-17 04:25
Subject: [MW:29843] Asme Section IX Thickness range qualification
Dear Experts,

I have some difficulty to interpret the requirements of ASME section IX

I have a  PQR Based on a dual process GTAW+SMAW ( 8 mm+17,4 mm) on an 25,4 mm butt weld.

Can I make a weld using only the GTAW process, base metal with a thickness of less than 5mm?

Are the image conditions correct?


wps77.png


Please give with details explanation regarding my above difficulty.


Thanks and Regards


Isac







--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c74dd763-9499-4097-b2cc-5cd52a84818d%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/973f737e-654a-43df-bf63-f84ed582caa9%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...