on my opinion support without saddle is a bad design. You get high stress concentration at the pipe

Στις Σάβ, 13 Ιουλ 2019 στις 7:33 μ.μ., ο/η harenath jha <harenathjha@gmail.com> έγραψε:
Please provide weld relief as per drawing. That's required

On Sat, Jul 13, 2019, 20:46 Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash

Can we provide the weld 

---------- Forwarded message ---------
From: Chiranjeevi A <chiranjeevipuvvula@gmail.com>
Date: Fri, 12 Jul, 2019, 11:10 PM
Subject: Pipe shoe support_urgent
To: <materials-welding@googlegroups.com>


Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0y03Qz6CxAPDB2qPk4_6EFXcfAuOSr4yu2cuLJf352%3D4g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UMafS9Tz7%3D6S4c5aM%2Beu%2B5MsjgbSswKeaAeBXvmF%2Batbg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40D4AV%2BRp%3DB1niepWyZTsfGij7MApPSSS8uMxv1jz9kHag%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...