Re: [MW:29843] suitable electrode for cast iron to ss 304

You can weld cast iron to steel using  Nickel electrode. The higher the carbon content, the lesser the weld ability. ... Cast iron is difficult, stresses are very high in weld , care to be taken , to weld.
Nickle electrodes such as Nickle 99 can be used . Check for joint design . Kindly See ANSI/AWS-A-5.15 .
Welding on cast iron may involves some repairs .

On Sat, 6 Jul 2019 at 20:17, 'prabir maji' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear all

I want to weld cast iron with SS 304, Kindly advice for suitable electrode SMAW process 

Thanking you,


P.K.MAJI
Sr Surveyor,
BUREAU VERITAS (I) PVT LTD.,
e-mail:-prabir.maji@in.bureauveritas.com
NAGPUR,
www.bureauveritas.co.in
Mob:9422127912

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20190706053128.27434.qmail%40f5mail-224-127.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OicGHmxKu3G0aStuKNdxGp4RiHOEbV%2BN%2BB%2BrEZnX9n2bw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...