Re: [MW:29831] Fwd: Pipe shoe support_urgent

Yes We Can provide, mouse hole shall be 25 mm away from weld on both sides

On Sat, Jul 13, 2019 at 7:16 PM Chiranjeevi A <chiranjeevipuvvula@gmail.com> wrote:
Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash

Can we provide the weld 

---------- Forwarded message ---------
From: Chiranjeevi A <chiranjeevipuvvula@gmail.com>
Date: Fri, 12 Jul, 2019, 11:10 PM
Subject: Pipe shoe support_urgent
To: <materials-welding@googlegroups.com>


Dear all,

can we provide the weld relief slot as per the below snap for pipe shoe support to avoid circumferential weld (Field weld joint) clash

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0y03Qz6CxAPDB2qPk4_6EFXcfAuOSr4yu2cuLJf352%3D4g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


--

Thanks and Regards,
Bathula Anil Kumar
SC:- 1873,
Phone number:- 99351283, 94350267

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD59513fEb%3DuuzvJq_Ty_zQP2%3DKeXm%3DRps_zYUoP_aHR%3DbzQew%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...