Re: [MW:29730] What grade of filler wire is to be chosen for MIG welding of 409M Ferritic Stainless Steel?

It's for structural purpose. 
Media - Atmospheric air (Structural Application).
Impact, tensile and hardness requirements needed.

On Tue, Jun 18, 2019, 9:43 PM Ramin Kondori <raminkondori@gmail.com> wrote:
What are your service requirements...?
Please provide us with the following:
  1. What are your design code or standards (ASME BPV, B31 series, etc.)
  2. Design temperature range, pressure range, etc. 
  3. What is your fluid or what are your corrosion requirements (media, CO2, H2S, any acids, etc.)
  4. Any specific mechanical requirements (impact test, tensile requirements, hardness, etc.)

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Thu, Jun 13, 2019 at 10:53 PM Ram <rameshsmit@gmail.com> wrote:
What grade of filler wire is to be chosen for MIG welding of 409M Ferritic Stainless Steel?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/85332ed1-a481-48b5-b76c-876db92dc2ed%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/DvcWjrEaCtk/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUis8GQ7v7NdhaBbifZDtwOgxm9Y784MuXE96%2BhR38gMSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPoWgWfryXAK_Xq7DQD8oT2eAHDLT6HicVzO-0gMy1TN6d7Ydg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...