Re: [MW:29724] Need Exact Electrode for Tool Steel

Selection of welding filler metals is a serious engineering process and requires knowledge and experience in material engineering and metallurgy, mechanical design and corrosion engineering (as a minimum). In short, you need to be a welding engineer to know how to select filler metals for any welding application.
  
In this case, E8018 series would be a general choice but you must consider the chemical composition and select matching filler metal composition (E8018/ER80S filler metals are not the same). Additionally, you need to know your Pre-heat & inter-pass temperatures and PWHT parameters. 

These all depend on the case. I recommend you to consult a qualified welding engineer. Doing these kinds of demanding jobs with online Q&A is not a good idea. 

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


On Sat, Jun 8, 2019 at 8:23 PM Venkatachalam Govindan <vinisaa@gmail.com> wrote:
Dear Sirs,

Anyone can help me to explain the method of electrode selection? for AISI 4130 and A681 L6 materials to weld for repair.

Also, please write about normal practice? 

Thanks and Best Regards,

Venkat. G

--
Venkatachalam Govindan
QHSE Lead / Trainer
(IRCA Registered Lead Auditor & API / CQI Practitioner)
+965 97604989, +919840502376 (
WhatsApp only)

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHOK3Oco1_4Gfzc0J5UVmNvT2kj62KMYFuHPeBkMahFQukHrOQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEagfUhbS8Dd3SdSPTT1VGVRMc2doqcP0F5%3DQhUC7nWGAGdz%2Bg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...