Re: [MW:29688] Possibility of Crack free in stellite 6 welding?

Sir why penning s not required in stellite? 

On Sun, 2 Jun 2019, 11:14 am Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
For stellite peening is not required

On Sat, 1 Jun 2019 10:28 pm Gopalakrishnan G, <gopal2408@gmail.com> wrote:
Thickness is 90mm and penning for stress relieving ( heat stress)

On Thu, 30 May 2019, 6:45 pm Kannayeram Gnanapandithan, <kgpandithan@gmail.com> wrote:
Why are you doing penning? Not 100%. crack free possible if the hardness is more than 35HRC. Why preheat

On Wed, 29 May 2019 9:34 pm Gopalakrishnan G, <gopal2408@gmail.com> wrote:
Dear experts 
 Whether  it is possible to achieve crack free in stellite 6 welding?

I have a job in which I have to carry out hardfacing by stellite 6 and buffer layer with Tenalloy (E-7016).Preheating carried above 350c and interpass 250c with penning and after completion of welding job is covered by heating blanket.
 When I carry out dye penetrant crater cracks appears. But my client needs with 100% crack free.plz kindly give ur valuable guidelines. Thk u.


Regards
G.Gopalakrishnan 
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKhugu9L6OHAss27tvndZhPOor%2BLHgGcBizCpiHe05O2uA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN8cQKX53Zu3HpXnYtE6dbhJwqhuSwYaJUW%2BU56eXNnJw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKgGUupqJwhNL8K%2BCGEggg_o_GWA09258H8%3DZgd4Qjp-Gg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNvq1%3Dimdk90Z7DUkku1MBX0W78%3DWCBJOPJztzLgv_o0Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKjUheqYij6-eku9Kn%3D_Z__ThE%3D8_OvSOc-bvhBVcMHcYQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...