Tuesday, June 4, 2019

Re: [MW:29681] ER70S-2 and ER70S-6 (GTAW Process)

Yes You can, Both "F" no are same

On Tue, Jun 4, 2019 at 10:50 AM 'HENNING John' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Yes you can.  However, if your WPS states that the filler metal per essential variable QW-404.5, will meet the Table QW-422 A-No. 1 chemistry limits, you will have to note that the Mn and Si must be 1.60 and 1.0 or less respectively.  You need to do incorporate this restriction as the SFA classification permits ER70-S6 to exceed the A-No. 1 limits

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of K K
Sent: Monday, June 03, 2019 5:40 AM
To: Materials & Welding
Subject: [MW:29673] ER70S-2 and ER70S-6 (GTAW Process)

 

Dear All,

 

My PQR is qualified with ER70S-2.

 

Can I use ( Mention) ER70S-6 in WPS.

 

Regards

Kiran

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/76403448-7204-4bda-83fd-21deebafcaa5%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/VE1PR01MB5678D8B47759DD02F3AF703E90140%40VE1PR01MB5678.eurprd01.prod.exchangelabs.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n-5nd9Z-qq4GVtfkM_mqxtK6SJ%3DgfhfXBhZTqMFBDDVQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...