Re: [MW:29628] Pipe sipport weld joint

Hi,

To contemplate on your scenario, after the butt weld of pipe to elbow, your construction team proceeded welding the shoe on elbow ? So as per your statement it is not just kissing with haz but clashing, which means your construction did intentionally, now you're here for correction.

Yes correction can be done as per your above proposal if your company has any standard stating with the clause or if you have a procedure or write and take approval.

One of world's top company standards clause waives your requirement with what you have proposed.

Check SAES-W-011, search for encroachment.

Thanks 

Muneeb

On Wed, May 22, 2019, 4:10 PM Chiranjeevi A <chiranjeevipuvvula@gmail.com wrote:
Dear George,

We are using ASME B31. 3

On Tue 21 May, 2019, 3:04 PM George Dilintas, <dilintas@gmail.com> wrote:
what is the applicable Code/ Standard (B31.1?, B31.3? other?)

Στις Παρ, 17 Μαΐ 2019 στις 12:18 μ.μ., ο/η Anil <chiranjeevipuvvula@gmail.com> έγραψε:
Dear All,

   In site we have one case that pipe shoe support weld clash with elbow weld, i.e.gap between weld toes is zero.

   Can we proceed with the joints at least 100mm of each welds will be tested with 100% X-ray, 100% VT and 100% MT

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8bd4bdfa-027b-44c6-96d8-b5bcee41de95%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40CYjz8qi%2Bmme2jva18Lh-5uF-gMm%3DUM%3DMuC%3DZdrhvOS-Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0yELuasmUicGpyssfy7Oa9UbCk3BwbwqLXhfoEZ4GFZqg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANtRWKu%2BLxVu7aVNUFfQBmcbqnHZtQ-AH7z4V-XSRFmLGMKPhg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...