Re: [MW:29609] Clad As per Sec IX




On Mon, 20 May 2019 at 17:39, K K
<karan.hbl@gmail.com> wrote:

Hi!

 For clad restoration you rrequire to qualfy for Overlay in the particular position as per ASME sex IX satisfying all overlay qualification requirement

For base metal welding you should  qualfy welder satisfying Sec IX Groove weld requirement

Regards

Hegde


Dear All,


We have three sort of clad,

 

CS + 825 clad pipe  (filler metal ERNiCrMo-3)

CS + 625 weld overlay pipe (filler metal ERNiCrMo-3)

CS + 316 clad pipe (filler metal ER 309 Mo)

 

As per ASME IX,  if welders need to be qualified in clad pipe or they can be qualified in CS regular pipes (QW-383)


Please give me your feedback.


Thanks and Regards

K K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7b831e8e-2e13-466d-abee-53248af13818%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1618970412.3194895.1558417866471%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...