Friday, May 24, 2019

[MW:29631] Re: Pipe sipport weld joint

dear Anil,
first of tell that with type of support is there. is it trunnion support, angle support etc.

if trunnion support is there then you can proceed with your weld and followed by NDT
you can proceed with the weld but take care while welding that there should be gap in welding of support whenever it collide with elbow weld.

don't weld on elbow weld. skip the welding on elbow weld. other place proceed with joint and do the NDT.

Thanks
Bhima Kanjariya


On Friday, 17 May 2019 14:48:39 UTC+5:30, Anil wrote:
Dear All,

   In site we have one case that pipe shoe support weld clash with elbow weld, i.e.gap between weld toes is zero.

   Can we proceed with the joints at least 100mm of each welds will be tested with 100% X-ray, 100% VT and 100% MT

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a9509674-639a-40d8-977e-ef86be689743%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...