Tuesday, April 9, 2019

[MW:29480] Welding of Hardened EN8

Dear experts,

Please help me in the following.
I want to weld hardened EN8 round bar dia 310mm to MS material.

Kindly suggest the electrode and care to be taken during welding.



--
Thanks and Regards,
Somnath Ashtakar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...