[MW:29464] Dual PWHT of SS410 after weld overlay of 625

Hi All,

Need your suggestion. 

Is it ok if we do Dual PWHT after 625 weld overlay on SS410 material. 

First PWHT- 685 for 8.5 hrs.
Second PWHT- 660 for 8.5 hrs.

Kindly suggest.