There are multiples way for the joining of aluminized or andoised steel only the process varies.

1. You can go for brazing and no need to remove the aluminium layer
2. If joining with GTAW, you need to pre-remove the AL layer in the welding areas.

With your question, I am not sure about the 
1. Coating thickness
2. Type of joint
3. Joint requirements or purpose of performing the welding


Thanks & regards
Sandeep Kumar

On Tuesday, March 26, 2019 at 5:28:56 AM UTC+3, Hrushikesh Sangamnerkar wrote:
Dear experts,

Does anyone has experience in welding aluminized stainless steel?

Grade is SS 347

If Yes, pl share
If No, share the reason

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...