[MW:29117] Re: Welding consumables certification

The certification requirements are laid down in  ISO 14344. The manufacturer is responsible for the compliance to the certificate and the manufacturer specify the quality requirements in their QMS. Now:
The welding consumable manufacturers provide filler wire with 3.1 for chemical i.e. actual results of the chemistry performed for each lot.

2.2 For mechanical properties which are typical values i.e. the stated minimum mechanical properties by the manufacturer.

In your case, you can ask the manufacturer to provide you 3.1 for chemical and mechanical both although it gonna cost to higher due to added cost to the manufacturer. Also it depends on your total requirements as for small qty. manufacturer may not entertain the requirements.


Thanks & regards
Sandeep Kumar

On Monday, October 5, 2009 at 1:49:51 PM UTC+3, ELAMARAN RAJAN wrote:
Dear Friends
 
As per our client specification for all welding consumables has to be minimum of EN10204 3.1 certification is required.
we are submitted EN10204 3.1 Chemical composition and for mechanical properties EN10204 2.2.
But Client not accepting that certificate due to mechanical properties has to be certified as per EN10204 3.1
 
let me know what is the difference between EN10204 3.1 and EN10204 2.2

regards
maran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...