Hi

With traditional welding process its not possible to weld AL with CS or HSLA. Although there are other possible alternatives available depending on job size and configuration, weldment properties required. such as

1. Brazing: Will give you the purpose of joining but lacks the strength
2. Friction stir welding: strength joint possible
3. Ultrasonic welding: strength joint possible
4. Adhesive bonding: strength joint possible
5. Using bimetallic inserts: strength joint possible

Above method need special joint preparation and may not suit what actually you mean by butt weld. Although, butt weld with special configuration can be made with specific process. E.g. a scarf joint for brazing or adhesive bonding. a bimetallic joint could be possible general butt joint configuration.


Thanks & regards
Sandeep Kumar


On Saturday, February 16, 2019 at 5:21:31 AM UTC+3, Ram wrote:
What is the filler wire used for joining High Strength Low Alloy Steel to Aluminium Alloy 5052 - H32? (Dissimilar welding - Butt joint).

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...