Re: [MW:28997] ASTM vs ASME for A312 N08926

ASME Section II adopts an ASTM standard.
Question 1: to which ASME edition you are refering?
Question 2: which ASTM edition do you have on hands? 

Στις Κυρ, 27 Ιαν 2019, 05:27 ο χρήστης Muhammed Ibrahim PK <ibratech@gmail.com> έγραψε:
Gents,

I received a pipe ASTM A312 N08926.
 
As per ASTM standard the Cr range required 24-26 and Nickel range 19-21.
As pr ASME standard the Cr range required 19-21 and Nickel range 24-26.

I have ASTM 2001 edition with me. Is there any updated edition available with changes?

Now it is confusing. Please advice your opinion on this.





Thanks & Regards
Muhammed Ibrahim PK

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...