Hello,

Acc. to AWS D1.1 2015
Plate: min. 180 mm in length, see 4.20.1 and figure 4.20
Pipe: OD less than and included 100 mm, full length; greater than 100 mm, a half pipe, see 9.22.2

Regards
Bien ND


Vào 21:28:59 UTC+7 Chủ Nhật, ngày 20 tháng 1 năm 2019, Darshan Revdiwala đã viết:
Dear Experts,
Can anyone confirm the welder qualifiacation RT length requirement as per AWS D1.1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...