Friday, December 14, 2018

Re: Re: [MW:28765] fillet weld , macroexammination , impact test

Q-1.. Single sided fillet weld is allowed for micro examination test for PQR testing ? if in drawing double fillet is given ?
Reply: NO
Q-2.. In macro examination beyond the root incomplete penetration and fusion is allowed ?
Reply: Visual or NDE fail dont go MACRO.
Q-3... Notch toughness  is also consider for fillet weld ?
Reply: QW-451.4 is identical to what stated in QW-170.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' - MUNEEB-
 
Date: 2018-12-13 11:13
Subject: Re: [MW:28762] fillet weld , macroexammination , impact test
asme sec 9 and astm 370

On Thu, 13 Dec 2018 at 08:18, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
In order to be able to help you, it is necessary that you specify which Code you are using to make these tests.

El mar., 11 dic. 2018 a las 23:26, Souravbohray (<ermechsouravbohray@gmail.com>) escribió:
Q-1.. Single sided fillet weld is allowed for micro examination test for PQR testing ? if in drawing double fillet is given ?
Q-2.. In macro examination beyond the root incomplete penetration and fusion is allowed ?
Q-3... Notch toughness  is also consider for fillet weld ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/JsrmacYc9kY/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...