Friday, December 28, 2018

Re: [MW:28821] WPS welding process dipostion

Hi Kumar

Your doubt  "how we decide filler metal diposition" i understand that , why used 13mm gtaw and 27mm smaw ? instead of other possibilities - right ?

There is no restriction in ASME Sec-9, You can  deposit any thickness you want and range qualified shall be as per table QW-451.1
Means in single test coupon, you can use multiple process and range qualified on your each process is based on WM thickness deposited.

This is the role of welding engineer to decide and prepare WPS/PQR to cover your current job and future job thickness requirements

i suggest to read QW-200 thoroughly 

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Thu, Dec 27, 2018 at 3:48 PM mithlesh kumar <mithleshmech47@gmail.com> wrote:
For ex- my PQR thk is 40mm qualified with 13mm gtaw and 27mm smaw. And wps base metal 5-200. So how we decide filler metal diposition.

Sent from my iPhone

On 27-Dec-2018, at 10:46 AM, Ramesh <rameshkannandevaraj@gmail.com> wrote:

Hi

Pl share minimum info like  PQR thickness, deposited Weld Metal thickness for each process in order to respond to your doubt.

What your WPS shows is the Base metal thickness range qualified, NOT individual process WM thickness range.

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Thu, Dec 27, 2018 at 10:36 AM Mohamed Muneeb <muneebslsa@gmail.com> wrote:
See if wps showing separately as per what has been written for each process in wps and the same applies you should follow the same.

If the case  your pqr has been qualified as per qw-452.1(b) and you want to go beyond that then you should rewrite your wps accordingly if your pqr qualifications for smaw has been recorded with  3 layers over with 13mm.

Read also qw-200.4.

Thanks.

On Thu, Dec 27, 2018, 10:18 AM mithlesh kumar <mithleshmech47@gmail.com> wrote:
WPS showing GTAW 20 mm and smaw 200mm and saw 200mm. From where in sec ix given for limit restrictions.

Sent from my iPhone

On 27-Dec-2018, at 8:58 AM, Mohamed Muneeb <muneebslsa@gmail.com> wrote:

No, limits restricted for each process as per wps.

Thanks

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 

On Thu, Dec 27, 2018, 8:28 AM Mithlesh <mithleshmech47@gmail.com> wrote:
Dear expert

WPS given thk range of 1.5-200 welding process given in wps is gtaw smaw and saw can we weld 200 mm with only smaw.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...