Re: [MW:28808] Material certification EN 3.1 OR 3.2 ?

Hi Ahmed,

The sentence or the clause or the snapshot might be intended for a ready stock material purchase.
It may be understood or considered as the mill test certificate is a 3.1 certificate and shall be endorsed with a TPIA-Inspector or Source Inspector (for visual, dimensional, chemical and and physical properties are verified as per material specification requirements (ASTM or API 5L spec or etc.) as an additional authentication for acceptance of the ready stock material.

So, the MTC will not be 3.2 certificate and it is 3.1 certificate.

With Regards
P Govindan

On Dec 24, 2018 1:39 PM, "shaikh ahmed" <ahmedmech77@gmail.com> wrote:
Dear Expert,

Please can you advise on below snap shot of Specification asking for EN 3.2 Material certification correct me ?

it calling for EN 3.2 OR 3.1



thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...