Dear,
First of all pl.  Mention the standard n grade of the pipe.  Refer the standard and look for dimensional tolerance as well.  Usually any wall thickness less than 87.5% of nominal is unacceptable...
Others correct me with other opinion..
Thanks,
Sk

On 10 Dec 2018 17:33, "Mohan" <ggnanamalli@gmail.com> wrote:
Hi Experts,

The piping pre fabrication work going in HRSG piping , in which it has been found that some of the 6" pipe to elbow welding for downcomer are not satisfactory. 


When investigated it was found that pipes, which has been supplied, there are some tool mark in inner surface(refer photo).


 When the thickness measured there is a reduction of 1.25 to 2 mm in thickness and in radiography a dark clear linear indication.


Whether it's acceptable, if its acceptable means suggest code reference 

or we have cut and re-weld


Regards

G Mohanraj

 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...