This topic seems quite interesting and I see divided opinions, I allow myself to give my opinion and if it is incorrect I hope that someone with more experience will give us more light and knowledge on this important topic.
Attached image of a part of a Welder Qualification, this was used for an ASME Audit, in other words it was reviewed by the ASME Authorized Inspector; two points:
1.- ASME IX works very differently than D1.1 does.
2.- In the column with red box: Range Qualified cross with Metal Base, there is a list of Numbers P (1 THROUGH 15F; 34 AND 41 THROUGH 49), I understand that the welder in this case was qualified for P1 with P1 but that has the ability and qualification to weld all P1 THROUGH P15F steels; P34 AND P41 THROUGH P49 and the combinations between these materials. It should be mentioned that this is suggested to the F-number, qualified position, thicknesses and diameters. in fact in an API course I heard that under ASME IX only three coupons are needed to qualify a welder in all materials, this if you do not take into account: F number, position, thicknesses and diameters. I will thank you infinitely for your contributions.

Libre de virus. www.avast.com

El jue., 22 nov. 2018 a las 22:25, muneebslsa@gmail.com (<muneebslsa@gmail.com>) escribió:
Greetings George,

It would be intresting if we know why it is not possible for this below case? with references, so that we can learn / adopt, your point of view, if it is acceptable.

Thanks.

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

(6:59) He has the keys to the realm that lies beyond the reach of human perception; none knows them but He. And He knows what is on the land and in the sea; there is not a leaf which falls that He does not know about and there is not a grain in the darkness of the earth or anything green or dry which has not been recorded in a Clear Book.

 
Date: 2018-11-23 00:35
Subject: Re: [MW:28660] Welder qualification
You cannot 

Στις Κυρ, 11 Νοε 2018, 04:19 ο χρήστης Surendra <skchordia.bhl@gmail.com> έγραψε:
Hello,

I have individual qualified welders per BPVC Section-IX-2015, as per following detail:

1. P1,G1 TO P1,G1

2. P8,G1 TO P8,G1

Can I use the same welder for welding of following?

1. P1,G1  TO P8,G1 

Thanking You,

Surendra
Bhilwara, Rajastha(Ind)


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza




Libre de virus. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...