1. Please refer AWS D1.1 , Part C for performance qualification requirements.

Range of qualifications - pl refer Table 4.10 & 4.11

 

2. Combination of WPS is allowed as per 3.6.1  This is applicable for both qualified or prequalified WPS.[ Screen shot from 2015 edition as below ]




Also refer OLD AWS interpretation as below [ 1984 edition]






Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Oct 31, 2018 at 10:06 AM Nithin Joseph <nithindsilva4u@gmail.com> wrote:
In AWS there is no provision of extracting a process. for eg, you are qualifying FCAW+SMAW, you have to use same combination on job too. Writing separate WPS for SMAW & FCAW is not acceptable as per AWSD1.1.

On Wed, Oct 24, 2018 at 2:11 PM shakin thobias <shakinthobias@gmail.com> wrote:
Dear experts

I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...