Re: [MW:28497] Combined PQR

what is the welding code?

On Wed, Oct 24, 2018 at 2:11 PM shakin thobias <shakinthobias@gmail.com> wrote:
Dear experts

I need to qualify welders in Both FCAW and SMAW. can i do both qualification in same PQR. what are the parameters and range of qualification. qualify that welders to max 30 mm thickness range. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Regards,
Nithin Joseph Dsilva
+971 557645785

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...