Upgrade of Mn and Ni from C3 to D1 and some differences in additional elements C3 has Cr Mo ranges....

Is this both belongs to same classification - Obviously NO.

Is this applicable as Non Essential Variable QW-404.12 ???

404.12 is mandated on covering supplementary essential, when falls for requalification becomes essential.

In your case you have asked commonly whether both falls under non-essential, for this answer NO and see the scnearios below.

E8018- D1 H4R to E8018- C3 H4R, in this case as per CVN requirements you can use but check the impact requirements.

E8018- C3 H4R to E8018- D1 H4R, in this case you simply cannot use, must requalification.

Regards,
Muneeb.M



 
From: Ri@z
Date: 2018-10-22 14:13
Subject: [MW:28477] Electrode Classification
Dear All,

E8018- D1 H4R 

E8018- C3 H4R 

Is this both belongs to same classification  ? 

Is this applicable as Non Essential Variable QW-404.12 ???



Riaz 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...