Re: [MW:28274] how to select filler metal for a specific Material according to ASME Sectionv IX

Please sir expalin about asme section ... how to select electrode

On Thursday, September 13, 2018 at 4:15:17 PM UTC+5, Tajuddin mohammed wrote:
Please kindly refer API 577 there is one table for selection of filler material 

On Wed, 12 Sep 2018, 16:47 adeel, <adee...@gmail.com> wrote:
Dear Experts,

Please answer this question 

For example designer selected a material SA517 Gr B for work.
 
I went to to table Q/QB 422 for P no. & G no. ... I found P no. is 11B and G no. 4. 

Then i went to Section ii Part A where i found SA 517 Material is alloy steel and its SFA no. is 5.5.

After that what shuould I do ?

 experts (Who has thorough of ASME Section IX) please tell me step  by step how to select exact filler material. from section ii part C.

I shall be very thankful to All of you for this act of kindness.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...