Re: [MW:28208] Minimize concavity of fillet weld in saw welding.

increase current and reduce travel speed. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Aug 23, 2018 at 11:53 AM Neem Lal <neem4u@gmail.com> wrote:
Dear All,

We are doing fillet welding of 10 mm leg length, so throat should be around 7 mm.
But due to concave weld profile we are getting 4 mm  to 6 mm throat.

What are the possible remedies to rectify this.


Regards

Neem Lal
Welding Engineer
HMM INFRA LTD.
AMBALA (HR) 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...