Wednesday, August 8, 2018

Re: [MW:28186] radiography to be consider for thinner plate or thicker plate

10 mm
Thanks,
Manoj

On Tue, Aug 7, 2018 at 12:40 PM Nadakuditi kiran kumar <kinnu78@gmail.com> wrote:
Dear Gentleman,
Please clarify the below doubt,
As per API 650 above 10 mm thickness shall be 100% radiograph to be
done for all T joints. When the joint between two dissimilar thickness
means 10mm & 12 mm what thickness we have to consider for radiography
whether 10mm or 12mm.

Thanks & Regards

N.Kiran kumar,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...