Thursday, May 17, 2018

Re: [MW:27854] can any suggest me regarding API 686

Hello Brother,

There is no certification/course for API 686.

Please be informed that API RP 686 is

"This recommended practice (RP), intended to provide recommended procedures, practices, and checklists for the installation and pre-commissioning of new, existing, and reapplied machinery and to assist with the installation design of such machinery for petroleum, chemical, and gas industry services facilities. In general, this RP is intended to supplement vendor instructions and the instructions provided by the original equipment manufacturer (OEM) should be carefully followed with regard to equipment installation and checkout. 

Most major topics of this RP are subdivided into sections of "Installation Design" and "Installation" with the intent being that each section can be removed and used as needed by the appropriate design or installation personnel".


Thanks,
Warm Regards,

Rajnish Dixit
Lead - QA-QC/QMS/Welding/NDT/Inspection
+91 972 4200 357

On Thu, May 17, 2018 at 7:24, Rameez khan RK
<rk.rameezkhan21@gmail.com> wrote:
Dear Expert ,


                can any one have knowledge regarding API 686 course and its material for preparation of API

Thank you

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...