Re: [MW:27703] Normalising

For simulating the condition cut PTC from formed dish. Incase manhole is there on dish, you can use the cutout as PTC otherwise remove material from extended straight portion of dish.

On Mon, 16 Apr 2018, 18:09 Jayesh Parekh, <jayeshparekh34@gmail.com> wrote:
If we do normalising to dish end, it's yield strength is increased due to strain hardening of dish end.. But this yield strength is restore by normalising. In normalising strength is reduced but after reduction it come to it's orignal yield strength. But if PTC undergone through same normalizing heat treatment, then it's yied strength is lower than Dish end yield Strength ?

material is SA516 gr-70.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...