Base metal welded                                                                                        Base metal qualified

Any one metal from P5A + Any one metal from P5A                       Any one metal from P5A with any one from P5A, P4, P3,P1

Any one metal from P15E to any one metal from any one Pno         Any one metal from P15E to any one metal from same welded Pno

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Apr 11, 2018 at 11:48 PM, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:
Two materials are mentioned in the original mail P5A and below in that mail mention P15E, I guess there is a confusion here, specifically I refer to the material P5A, THAT WAS THE POINT THAT I EXPOSE.
Please see attached image.



Hi 

This is Srinivas, 

I got a PQR P5A to P5A , So i can write WPS P5A to P4 from that P5A to P5A PQR ? 

Based on QW 424.1 ? 

On Sunday, 6 April 2014 12:18:17 UTC+8, Binoy Lonappan wrote:
As per Section IX QW 424 for procedure qualification it is given thatt 

for base material range of qualification as P15 E metal to P4 metal is 
qualified for any metal from P15E to P4 or P3,P1 
But P number is an essential variable so what is the actual 
interpretation of the above clause 

Or does it means if we qualify procedure for P15E +P4 then it is 
qualified for the P15E any metal from this group to any metal from 
P4,P3 P1 groups



2018-04-11 9:04 GMT-05:00 George Dilintas <dilintas@gmail.com>:
You have to read QW 403.1 and then QW 424 carefully. Your interpretation is wrong . If your PQR was done using a P15E and a P4, then you can support WPS which are for any P15E to any P4 ONLY

2018-03-28 10:38 GMT+03:00 srinivas <srinivasduraisamy@gmail.com>:
Hi 

This is Srinivas, 

I got a PQR P5A to P5A , So i can write WPS P5A to P4 from that P5A to P5A PQR ? 

Based on QW 424.1 ? 

On Sunday, 6 April 2014 12:18:17 UTC+8, Binoy Lonappan wrote:
As per Section IX QW 424 for procedure qualification it is given thatt

for base material range of qualification as P15 E metal to P4 metal is
qualified for any metal from P15E to P4 or P3,P1
But P number is an essential variable so what is the actual
interpretation of the above clause

Or does it means if we qualify procedure for P15E +P4 then it is
qualified for the P15E any metal from this group to any metal from
P4,P3 P1 groups

--
With Regards
Binoy Lonappan
+91-9645100560
QAC Engineer
TECCL

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--

Ing. José Juan Jiménez Alejandro

ASME Independent Consultant 

and Technical Manager SSI-TPI

Cel. +52 812 352 4606

Skype: jjjimeneza

Twitter: @jjjimeneza



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...