Hi Manoj ,

Yes its possible and ok to do a water fillup test after painting , but pls ensure that the painting has been given required curing time to avoid any cohesive disbandment .

Regards,
Pratish 

On Monday, April 23, 2018 at 3:52:28 AM UTC+1, John Manoj wrote:
Dear expert.

We have one proposal to do water fillup test after internal and external painting of water tank which is fabricated as per API 650.
Internal paint : 300 micron  polyamine cured novolac epoxy coating.
External : 205 micron paintining.

Is it possible to do water fillup test after painting,

Thanks in advance,
Manoj.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...