Monday, March 26, 2018

Re: [MW:27571] PQR (B31.3 vs B31.1)

Hi 

 

Pl refer ASME B31.1 , Chapter V – Clause 127.5 Qualification

 

Even though your construction / design code is ASME B31.1,  PQR requirements are as per Sec IX only..

 

You can use that PQR provided  if there is no specific additional testing requirements by client.









On Mon, Mar 26, 2018 at 6:55 AM, 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear 
PQR is as per ASME SEC IX not as per B 31.3.
So that you can use any where for P No 1.

Regards 
A P GUPTA 
IOCL BARODA
THYSSENKRUPP 



On Sat, 24 Mar 2018 at 10:07 PM, 'Maghroud Moussa' via Materials & Welding

Dear experts.

I have a PQR for P1 (GTAW, PWHT)qualified with Sec IX and B31.3. Is this PQR can used to supporte PQR in a power plant project that the code is B31.1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...