Dear 
PQR is as per ASME SEC IX not as per B 31.3.
So that you can use any where for P No 1.

Regards 
A P GUPTA 
IOCL BARODA
THYSSENKRUPP 



On Sat, 24 Mar 2018 at 10:07 PM, 'Maghroud Moussa' via Materials & Welding
<materials-welding@googlegroups.com> wrote:

Dear experts.

I have a PQR for P1 (GTAW, PWHT)qualified with Sec IX and B31.3. Is this PQR can used to supporte PQR in a power plant project that the code is B31.1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...