Hi 

This is Srinivas, 

I got a PQR P5A to P5A , So i can write WPS P5A to P4 from that P5A to P5A PQR ? 

Based on QW 424.1 ? 

On Sunday, 6 April 2014 12:18:17 UTC+8, Binoy Lonappan wrote:
As per Section IX QW 424 for procedure qualification it is given thatt

for base material range of qualification as P15 E metal to P4 metal is
qualified for any metal from P15E to P4 or P3,P1
But P number is an essential variable so what is the actual
interpretation of the above clause

Or does it means if we qualify procedure for P15E +P4 then it is
qualified for the P15E any metal from this group to any metal from
P4,P3 P1 groups

--
With Regards
Binoy Lonappan
+91-9645100560
QAC Engineer
TECCL

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...