[MW:27578] Re: PQR (B31.3 vs B31.1)

Dear

If project spec. simply says only ASME Sec. IX on welding qualification requirements, you can use the PQR as it is.

Suppose, project spec specifies any additional tests during PQR, then you have to go for new PQR incorporating all project specific variables / requirements.

B31.1 OR B31.3 does not deal with any welding qualification requirements.

Regards

R Vairamuthu


On Saturday, March 24, 2018 at 7:37:06 PM UTC+3, Maghroud Moussa wrote:

Dear experts.

I have a PQR for P1 (GTAW, PWHT)qualified with Sec IX and B31.3. Is this PQR can used to supporte PQR in a power plant project that the code is B31.1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...