Of course... it is acceptable...


Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        

On Thu, Jan 25, 2018 at 4:28 PM, 'DOKKU AJAY' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Gents,

I have the following query. Appreciate if someone can guide on this:

Background: 
Cladded Vessel, Nozzle of Size 2", MOC: CS+SS Cladd/ Overlay, Code of Construction: Sex.VIII Div.1 : Vendor confirms that they cannot do weld overlay of 2" and less size. Alternative confirmed by vendor is to machine the Forged Bar to make 2" SS Pipe. Our Engineering has accepted the replacement of material from engineer point of view i.e from CS+SS Overlay to SS Matl.

Query:

Is it acceptable from code point of view to used forged item for manufacturing of Nozzle pipe.

Regards,

Ajay Kumar Dokku


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...