Re: [MW:27294] SS Forged Bar machined to make Pipe for Nozzles Fabrication

Procurement confirms non availability of pipe matl readily and the lead time will be 12 weeks.


On Thu, Jan 25, 2018 at 5:06 PM, Raghuram Bathula
<raghurambathula@gmail.com> wrote:
why don't use pipe?

On 25 January 2018 at 16:58, 'DOKKU AJAY' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Gents,

I have the following query. Appreciate if someone can guide on this:

Background: 
Cladded Vessel, Nozzle of Size 2", MOC: CS+SS Cladd/ Overlay, Code of Construction: Sex.VIII Div.1 : Vendor confirms that they cannot do weld overlay of 2" and less size. Alternative confirmed by vendor is to machine the Forged Bar to make 2" SS Pipe. Our Engineering has accepted the replacement of material from engineer point of view i.e from CS+SS Overlay to SS Matl.

Query:

Is it acceptable from code point of view to used forged item for manufacturing of Nozzle pipe.

Regards,

Ajay Kumar Dokku


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...